Medium Impact Grade. Medium Impact Strength Low Residual Monomer, Good Heat Resistance, Base Color Stability,, Good Transparency, Easy Processing ,High Flow , High Gloss
|
Properties |
ASTM method |
Test Condition |
Unit |
Typical Value |
|
Specific Gravity |
D542 |
--- |
--- |
1.046 |
|
Melt Flow Index |
D1238 |
200°C,5 kg load |
g/10 min |
4.6 |
|
Tensile Strength at Yield |
D638 |
23°C,1/8” Sample |
kg/cm2 |
300 |
|
Elongation at Break |
D638 |
23°C,1/8” Sample |
% |
40 |
|
Izod Impact Strength |
D256 |
23°C,A method,notched1/8”×1/2”×5/2” |
kg/m2 |
9.5
|
|
Vicat Softening Temperature |
D1525 |
1 kg load,3 mm Thick ( 120°C/hr ) |
°C |
97 |
|
Flammability |
UL-94 |
1/16” Sample |
File No.E50263 |
94HB |
|
Residual SM monomer |
--- |
--- |
ppm |
<300 |
|
Yellow Index |
--- |
--- |
--- |
-6 |
Our factory